Peroxide Fluxer
The best results call for the best solution
Prepares : Solutions for AA, ICP and wet chemistry analysis
Specially designed for: Fusing samples in sodium peroxide, sodium carbonate and potassium pyrosulfate
Processes :
- Highly refractory compounds such as chromite, magnetite, ilmenite, rutile, silicon and silicon carbide
- Materials with high sulfide contents
- Noble metals
- Use of zirconium crucibles
- Complete dissolution of the sample; even the toughest refractory material
- Retention of volatile elements
- Reduction of acid impurities
- All fusion parameters can be modified: heating duration, mixing speed & amplitude, gas flow, etc.
- Fully automatic
- Preset fusion programs available
- Easy loading of zirconium crucibles
- NO manipulation of HF acid, pressured vessels and hot labware
- Individual burner selection
- Propane or natural gas powered
- Saves time: 5 - 10 minutes to prepare a solution
- High throughput: 6 samples at a time; 40 to 60 samples per hour
- One burner-per-sample design
- NO compressed air, NO oxygen required
- Low maintenance and repair cost